Hot
Features of IFUN Denture Base Resin(3166 )
Highly biocompatible safe to allergic patients.
It has high biocompatibility with oral tissue. Ensure a healthy oral environment and a high degree of comfort.
Excellent mechanical properties.
The denture base printed with our 3166 resin are durable and resist fracture
Excellent mechanical properties.
The denture base printed with our 3166 resin are durable and resist fracture
- Post Processing Steps
-
1- Washing
– After the printing is completed, wash the part as attached to the building plate with alcohol (>%95) for 3 minutes.
– Make sure that alcohol covers the part entirely when washing.
– Since the Denture resin is biocompatible never wash it with the alcohol used for other resins before.
– Use a brush to remove uncured resin if needed.
– Do not over-wash, it may cause deterioration in dimensions of the part.2- Drying
– Use air-compressor to dry the washed part.
– Make sure that the part is dry and uncured resin is cleaned up completely.
– If still uncured resin left on the part, wash it with fresh alcohol and dry again.3- Part Removal
– Remove the printed part from the building plate using a scraping tool.
– Be very careful not to damage the model.4- Post Curing
– UV post-curing for 5 minutes
–
After the post curing, supports should be removed from the model
cautiously and then desired sandblasting and polishing can be done
project | Content | Data value | Testing method |
Physical and
chemical properties (before curing) |
color | Pink | |
Viscosity | 450-750cps(25℃) | ASTM D1084-1997 | |
Density | 1.05-1.15 | ASM D1875-69(1980) | |
Physical and
chemical properties (after curing) |
Curing depth | 500~700μm | |
Shrinkage | <1% | ||
Hardness | 70~80D | ASTM D2240-05(2010)
|
|
bending strength | >3kg | . |